Mito57
Mechanical
- Feb 21, 2005
- 13
We have a 650 tank which already has been a second floor installed on top of the original following API 653. We installed a leak detection system between the two floors and lately it was noted that there was a leak. Tank was internally inspected and we are considering a new floor replacement.
Somebody put on the table the idea of installing a 3rd floor on top of the other two. I have looked at the Code and did not find anything against this if all previsions are followed. Still I don't feel 100% comfortable with the idea because I think this 3rd floor may lack proper support.
Due to the nature of the contents that have leaked between the two floors there is some concern on welding to the second floor. This is the reason why this idea was presented.
Anybody had done this before? Any feedback?
Somebody put on the table the idea of installing a 3rd floor on top of the other two. I have looked at the Code and did not find anything against this if all previsions are followed. Still I don't feel 100% comfortable with the idea because I think this 3rd floor may lack proper support.
Due to the nature of the contents that have leaked between the two floors there is some concern on welding to the second floor. This is the reason why this idea was presented.
Anybody had done this before? Any feedback?