API 650 11th Edition Section 7.2.3.2: The upper plate at a horizontal butt joint shall have a 4:1 taper when its thickness is more than 3 mm (1/8 in.) greater than the lower plate.
When would the upper shell plate be thicker than the lower plate?
Does API offer guidance when the lower plate is more than 1/4" thicker than the upper plate?
When would the upper shell plate be thicker than the lower plate?
Does API offer guidance when the lower plate is more than 1/4" thicker than the upper plate?