Hello everybody,

I would like to know the minimum thickness of the bottom plate of an athmospheric storage tank. What does API 650 say?

Thanks for any reply

UliR
 
API 650 minimum bottom plate thickness is 1/4" [6mm] exclusive of any corrosion allowance, and 72" [1800mm] in width.
 
Hello IFRs,

thanks for your fast and helpfull reply.

Greetings from Cologne in Germany

UliR
 