Is it permissible (or is it prohibited) to Machine a 9" Valve (Flanged) body from a Forged Cylinder of 500mm dia and 200 mm high or a forged cube of 450mm side?
Is it mandatory to forge the component as close as possible to final shape or is it permitted to machine the part from a forged cube or forged cylinder.
If there is a prohibition, request you to provide me the reference clause of API 6 A.
Material under discussion is AISI 4130.