Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations KootK on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

API 5L X60 SEAMLESS THICKNESS LIMIT

Status
Not open for further replies.

GabrieleB

Petroleum
Feb 4, 2009
84
Somebody could indicate me which is the commercial thickness limit for API 5L X60 seamless? Is possible to find pipe with 22 mm thikness seamless? Thank in advance for your help
 
Replies continue below

Recommended for you

GabrieleB

22mm is not a standard API 5L thickness. Check the tables in API 5L.

If you need 22mm (.866") then you are faced with 2 choices use the next standard API 5L size, which is 22.225mm (.875") or ask for a special run of pipe, which unless you have hundreds of kms, it probably won't be worth it.

Greg Lamberson, BS, MBA
Consultant - Upstream Energy
Website:
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor