In API 16A Sec. 7.3.6.2 "Deposited weld metal properties" it states: The deposited weld metal mechanical properties shall meet or exceed the min specified mechanical properties of the base material. Verification of properties shall be established through the implementation of the manufacturer's WPS and supporting PQR. When materials of differing strength are joined, the weld metal shall meet the minimum requirements of the lesser material.
What does this mean? Does this say that when I develop a new WPS and PQR that I must do mechanical testing with specimens made from strictly weld metal along with the specimens of base and weld metal? Or is the required mechanical testing of the welded specimens enough?
What does this mean? Does this say that when I develop a new WPS and PQR that I must do mechanical testing with specimens made from strictly weld metal along with the specimens of base and weld metal? Or is the required mechanical testing of the welded specimens enough?