Airarc
Petroleum
- Mar 17, 2013
- 2
In the Api 12f weld definitions it describes a double weld butt joint with a note stating it's equivalence can be achived with one side welded with complete penetration.
In section 5 it states all weld joints require welds on both sides.
Question I have would one side welding with complete penetration be allowed.
Any advice would be helpful.
Airarc
In section 5 it states all weld joints require welds on both sides.
Question I have would one side welding with complete penetration be allowed.
Any advice would be helpful.
Airarc