Hi, refer to the API 1104 - Clause 6 Qualification of Welders.
1. If a welder passed 5G qualification, what is the tolerance (degree) for the horizontal production welding?
2. What is 6G (tolerance of degree) during the production welding?
I noticed that no further details in the API1104, shall we need to refer to ASME IX with regards to the position?
1. If a welder passed 5G qualification, what is the tolerance (degree) for the horizontal production welding?
2. What is 6G (tolerance of degree) during the production welding?
I noticed that no further details in the API1104, shall we need to refer to ASME IX with regards to the position?