It is an essential variable electrode polarity for the welder?
 
Replies continue below

Recommended for you

Within other restrictions of API 1104 Section 6.2.2, a change in polarity is not an essential variable for welder qualification. It is, however, an essential variable for welding procedures (API 1104 5.4.2.7).
 