Hello i have two questions concerning essential variables within API 1104, 21st edition Sep 2013:
1st question:
As per 5.4.2.1 a change in the welding process or method of application has to be considered
as an essential variable.
What does method of application mean?
Only a change from manual to automatic or semiautomatic,
or as well the type of beads e.g. stringer, weaver?
2nd question:
As per 5.4.2.3 a major change in joint design has to be considered as an essential variable.
Further, minor changes in the angle of bevel or the land of the welding groove are not essential variables.
A PQR indicates a butt weld with a landing/root face of 2mm.
Now, I want to establish a WPS indicating a butt joint without a landing/root face, has this to
be considered as a major change in the joint design?
Thank you for your help
Joerg
1st question:
As per 5.4.2.1 a change in the welding process or method of application has to be considered
as an essential variable.
What does method of application mean?
Only a change from manual to automatic or semiautomatic,
or as well the type of beads e.g. stringer, weaver?
2nd question:
As per 5.4.2.3 a major change in joint design has to be considered as an essential variable.
Further, minor changes in the angle of bevel or the land of the welding groove are not essential variables.
A PQR indicates a butt weld with a landing/root face of 2mm.
Now, I want to establish a WPS indicating a butt joint without a landing/root face, has this to
be considered as a major change in the joint design?
Thank you for your help
Joerg