Just as the title says... any hints?
 
Replies continue below

Recommended for you

Matweb lists it here with a button for supplier links:

Supplier listed is: Stern & Co. Inc. is a distributor of plastic resin and sheet. We specialize in polystyrene, polypropylene, polyethylene, ABS, SAN, and PET. We inventory prime and widespec resins nationwide. We sell hips, coex, pet, rpet, and pp sheet and rollstock. To locate a sales office close to you, please call us at 732-382-9666, or fax us at 732-382-0054. You can visit our web site at
Or call INEOS for a list of their distributors. Or, as ABS is a commodity, use MatWeb to find an alternate grade from Dow, BASF etc..

Chris DeArmitt

Expert consulting & training
 
Thank you! Very helpful materials website...
 