This material is now depreciated - replaced by 7055-T76511 I believe. Anyway, working with a legacy installation and need to find those material properties. I understand it's in older versions of MIL-HDBK-5.

Anyone got data for this?

Thanks,

Joe

--
Joseph K. Mooney
FAA DER Structures
 
joekm,

Non current Mil-Hdbk-5 Revison D, dated June 1983 has the allowables for 7178 in it. I have a pdf file of this section. Please send me contact information if you would like this file.

Regards
 
Thanks MNLiaison, you can reach me at joekm@verizon.net

Regards,

Joe

--
Joseph K. Mooney
FAA DER Structures
 