Does anyone know any type of paint/primer/whatever that can be sprayed on top of carbon fabric, without altering the resin infusion properties and mechanical properties (fiber/resin adherence, resin strength, and so on...)? I would like to "draw" the shape of the carbon/epoxy samples on top of the laminate before the infusion, in order to make the cutting process easier. I hope my question is clear enough... ;-) Thanks in advance!
Does anyone know any type of paint/primer/whatever that can be sprayed on top of carbon fabric, without altering the resin infusion properties and mechanical properties (fiber/resin adherence, resin strength, and so on...)? I would like to "draw" the shape of the carbon/epoxy samples on top of the laminate before the infusion, in order to make the cutting process easier. I hope my question is clear enough... ;-) Thanks in advance!