There's known issues about pitting corrosion occuring on our anti-icing tubes on the air intake heat exchanger units fitted on our gas turbines. These operates at above 420degC.
Before i kick off this into a big project in replacing all our tubes with materials with better Pitting Resistance Equivalent number (PRE). I have done my own initial research and drafted the following;
Corrosion source/type: sulphur from neighbouring plant polution, atmospheric assisted corrosion.
Questions:
. Is coating/painting a suitable remedy for these tubes?
. As anyone experienced same issues and how did they deal with it?
. How do you mitigate against sensitization?
. What material is best for tubes operating over 420degC to resist sensitization and has high PRE?
Deduction
My deduction was items with high melybdenum and chromium content i.e. one of the following:
SA-312 TP316L : 16Cr-12Ni-2Mo (Pipe)
SA-213 TP316L : 16Cr-12Ni-2Mo (Tube)
SA-268 SA4735 : 29Cr-4Mo (Tube)
SA-249 SA4400 : 18Cr-2Mo (Tube)
Please advise
Thanks
Please do drop more information or knowledge you have on this subject they will all be taken in and appreciated.
David O.
Mechanical Engineer
Graduate as of: 2007
Oil, Gas & Power
Before i kick off this into a big project in replacing all our tubes with materials with better Pitting Resistance Equivalent number (PRE). I have done my own initial research and drafted the following;
Corrosion source/type: sulphur from neighbouring plant polution, atmospheric assisted corrosion.
Questions:
. Is coating/painting a suitable remedy for these tubes?
. As anyone experienced same issues and how did they deal with it?
. How do you mitigate against sensitization?
. What material is best for tubes operating over 420degC to resist sensitization and has high PRE?
Deduction
My deduction was items with high melybdenum and chromium content i.e. one of the following:
SA-312 TP316L : 16Cr-12Ni-2Mo (Pipe)
SA-213 TP316L : 16Cr-12Ni-2Mo (Tube)
SA-268 SA4735 : 29Cr-4Mo (Tube)
SA-249 SA4400 : 18Cr-2Mo (Tube)
Please advise
Thanks
Please do drop more information or knowledge you have on this subject they will all be taken in and appreciated.