The shop has heat treated a batch of parts made of 2024-0 alclad .032" thick to T4 temper. The parts were not correctly formed and we want to anneal the parts, correct them and then re-heat treat to T4. What temp do we heat them to, how long to soak and length of cool down. Any help?
 
Replies continue below

Recommended for you

SAE-AMS-2770
Old revision MIL-H-6088. Available Free.

Are you sure they didn't warp during Heat Treat?
 