Tippy1

Materials
May 20, 2003
1
What conditions should I use to achieve the maximum softness for SAE 1006 steel. I want to get it below 50 Rockwell .
 
Replies continue below

Recommended for you

Check out the following thread, and the other thread that is referenced within it:

thread330-47316
 