Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

AN-QQ-S-752 1

Status
Not open for further replies.

brin

Aerospace
Mar 12, 2000
122
does anyone have a copy of AN-QQ-S-752? I've tried DODASSIST, IHS, etc. and am getting desparate.

thanks
 
Replies continue below

Recommended for you

Hi Brin,

I don't have QQ-S-752. It looks like one of those ancient specs superseded long ago. Typically, you need a historic document subscription in IHS to get access to these. I had one at one time because I worked with 727's and DC8's.

If you follow the link below, you will be able to see that QQ-S-752 is 4140 steel. If you need material properties or current AMS spec info, you could look in MMPDS.

Hope this helps.

 
thanks for the link, I've never come across that figmat.pdf document before.

IHS.com and all the other standards repositories do not have a lot of the AN-QQ-XX-XXX specifications. If anyone has someplace else to try I'd like to hear about them.

 