Hi all,
Does anybody know a link to show me the following standard?
AMS 6504

 
You will have to buy it or find a library that payed for it. Only MIL-STD's are free on the web.
 
Does anybody know its composition?
 
Are you sure that this is AMS 6504? I did a search on Google and other search databases and didn't find any mention of such AMS standard. I searched MIL-HDBK-5J and ASSIST-QuickSearch too and didn't find anything so I assume it is not a spec for an aerospace metal. Can you give info what it dealing with (Materials, Metals, Testings, Coatings etc.)?
 
There is no standard SAE AMS6504. Please confirm the designation that was given to you.
 
AMS5604 ???
Steel, Corrosion Resistant, Sheet, Strip, and Plate 16.5Cr 4.0Ni 4.0Cu 0.30Cb, Solution Heat Treated, Precipitation Hardenable

Abstract: This specification covers a corrosion-resistant steel in the form of sheet, strip, and plate.

These products have been used typically for parts requiring corrosion resistance and high strength up to 600 degrees F (316 degrees C) and where such parts may require welding during fabrication, but usage is not limited to such applications.

Certain processing procedures and service conditions may cause these products to become subject to stress-corrosion cracking; ARP1110 recommends practices to minimize such conditions.
 