Oct 29, 2013 #1 Dougt115 Mechanical Joined Oct 2, 2013 Messages 197 Location US Where can I get a copy of AMS 2759? I am looking for the hydrogen embrittlement baking information on 17-4 H900 SST with hard chrome plating (HRC 43-46).
Where can I get a copy of AMS 2759? I am looking for the hydrogen embrittlement baking information on 17-4 H900 SST with hard chrome plating (HRC 43-46).
Oct 29, 2013 #2 TVP Materials Joined Apr 12, 2002 Messages 4,592 Location US Here http://standards.sae.org/ams2759/9/ or here http://global.ihs.com/search_res.cf...d=21254B2B3D0A&country_code=US&lang_code=ENGL Upvote 0 Downvote
Here http://standards.sae.org/ams2759/9/ or here http://global.ihs.com/search_res.cf...d=21254B2B3D0A&country_code=US&lang_code=ENGL