AMS 2689

Status
Not open for further replies.

brin

Aerospace
Mar 12, 2000
122
I'm looking for a company that can weld and certify to AMS 2689 fusion welding for Titanium.

So far we haven't found anyone who can do this and things are getting desparate. Any suggestions?

Thanks
 