An ammonia condenser has well water as cooling media on the tubeside. Condensing Ammonia on the shell side. After just ~6 years in service, tube leaks developED. Obvious first hand solution was to plug the leaking tubes with tapered plugs. Now during retubing, if you try to drill out the plug, existing pressure is noticed behind the plug! why is that? what is the mechanism for this to happen? Theoretically, leaking tubes should release to atmosphere when the exchanger is depressurized.