Sep 16, 2004 #1 djoko Chemical Joined Jan 3, 2003 Messages 10 Location ID do anybody know where i can find that?? thanks
Sep 22, 2004 #2 SAE79 Chemical Joined Sep 22, 2004 Messages 2 Location US Al(OH)3 alumina trihydrate has a heat capacity of approximately 0.24 BTU/lb*deg F. AlF3 (aluminium trifluoride)should have a comparable value. I am not familiar with aluminum trifluoride trihydrate. Upvote 0 Downvote
Al(OH)3 alumina trihydrate has a heat capacity of approximately 0.24 BTU/lb*deg F. AlF3 (aluminium trifluoride)should have a comparable value. I am not familiar with aluminum trifluoride trihydrate.
Sep 23, 2004 Thread starter #3 djoko Chemical Joined Jan 3, 2003 Messages 10 Location ID sae79... i mean AlF3.3H2O aluminum fluoride trihydrate. sorry for the wrong name and thank you for your info. djoko Upvote 0 Downvote
sae79... i mean AlF3.3H2O aluminum fluoride trihydrate. sorry for the wrong name and thank you for your info. djoko