I have an application that calls out aluminum tubing 2024 per QQ-A-225-6.
The size is 1.3125 od x .755 ± .0025.

Can anyone tell me if this is a common size? Is this a special make?

Is there a place where I can get this material? I cannot seem to find it.

THANK YOU
CNCMILL
 
the ID looks decidedly funny (unless it's a stammer)
 
Your right I might need to go back and double check. Thanks.

Thank You
CNCMILL :-)

 
The "QQ-" specification was superseded back in 2004 eventually being replaced by ASTM B 211.
 
JFSSWISS

For extruded tube [which is what you actually described] specify: 2024-(temper) per AMS-QQ-A-200/3 [extruded BAR, ROD, SHAPES, TUBE AND WIRE]

CAUTION: If these materials are for NON-AEROSPACE use, then the ASTM equivalent material is "OK". Otherwise... stick to the AMS material!!!!!!

Regards, Wil Taylor
 