In the past I have always specified using 6061-T6 alloy for the entire handrail. Someone has recently told me that they do not make any of the bends out of the 6061-T6, and instead use 6061-T4 alloy. This is the first time I have seen it and was wondering if anyone else had come across this. Is it common?

Thanks,
Michele
 
Replies continue below

Recommended for you

Work out if it's possible to make the bends you specified with 8 pct elongation.



Mike Halloran