Hi...i'm working on a proyect and i need to know the aluminum alloys that are usually used on the engine blocks and heads..any information on this issue would be appreciated...Thank you.


José Luis Walters.
 
for sand cast components, alloys 356/A356 are used for blocks, and 319 for heads.

for die cast components, alloys like 380 and 390 are used.
 