Tried searching google but struggled to find any information.

I am familiar with the standard aluminium extrusion process for constant section. I am wondering if there is a possibility to extrude a section lets say circular starting at 100mm diameter reducing to 75mm over an 8m length, maintaining a 5mm wall thickness.

I would be interested to know if this is possible and any references to the die design to achieve this.
 
with sailboat masts they do but I don't know the tolerances
 
Tapered aluminum tube is a thing.

It may begin as straight extruded tube.

Then tapered by other processes.

Constant wall thickness is probably hard.
 
I have seen progressive forming of masts then welded, but never seen a tapered extrusion.

I have noticed reference to variable geometry dies so was curious if this is actually possible.
 
engineeringspread,

A tapered tube sounds like a good application for welded sheet metal. The 5086 grade is fairly strong in the as-welded condition.

--
JHG
 

I called a leading UK extruder and was informed this process is not one they are aware of, so my guess is this isn't possible.
 