Hi there,

We want to build a cooling shell to get as close as possible to our cooled elements (step shape). It is made of aluminium plates (~20mm thick) bolted together. They will be drilled with two holes each.

There is no much space in the front, so the idea is making a pocket to connect the two holes and then well a cap to close it. On the back we use pipes with a U shape. Here some pictures of the idea:
Cooling_shell_01_qre7xs.jpg

Cooling_shell_03_lcral4.jpg

Cooling_shell_02_bz0tnh.jpg

Cooling_shell_04_ldtd6c.jpg


There is a new proposal to simplify the manufacturing process. Drilling the two holes not through (almost to the end), then perpendicularly from a side make a third hole that connects the two firsts, and then using a cap (which could be even a screw-like cap). I understood this second idea is used in plastic injection moulds.

We use alcohol for cooling (-25ºc/-13ºF).

Cooling_shell_10_k1jn9j.jpg

Cooling_shell_11_ujuxwq.jpg

Cooling_shell_12_odwo8z.jpg


The second option is easier to build, but I fear the coolant can get in the screw-cap threads gaps and corrode more. If we weld a cap there will be a dead-end.