Hi everyone,

does someone know where to find some altymid plates, ageing tests (lifetime) and prices?

we need a lifetime of 8 years at 300°C in ambiant atmosphere, do you think this high temperature polymer could bear these high temperature?
 
Replies continue below

Recommended for you

Thank you for yourhelp... That was the first thing I read... I'm looking for more useful information...
 

As a guess, as the max temp stated is 315 (or 317)deg C, I would assume that is for short term excursions rather than continuous. It is probably also under zero stress.

Cynic? Moi?

To answer your question - probably not.

H
 
That confirms what I was thinking, but I have no proof for that, and I have to justify my choices on facts... Celazole is really better, but what an expensive price!
 
So what's wrong with Al ceramic or Steel?

H
 
Have you tried calling DuPont. They came up near the top of my first google search as a manufacturer of polyimide.

They normally supply excellent technical support.

They can certainly recommend a converter to you from their customer list.

Regards

eng-tips, by professional engineers for professional engineers
Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor