Dec 1, 2005 #1 morojlu Mechanical Joined Nov 12, 2004 Messages 20 Location IR Hi all, What's The main difference between A335-P22 CL.1, CL.2 AND CL.3 regards, Mehdi Orojlu
Dec 1, 2005 #2 NozzleTwister Mechanical Joined Mar 3, 2003 Messages 368 Location US Where did you get these Class designations? To my knowledge there are no Class designations associated with A335-P22. Nothing is mentioned in the current ASTM standard for this material. Please advise. NozzleTwister Houston, Texas Upvote 0 Downvote
Where did you get these Class designations? To my knowledge there are no Class designations associated with A335-P22. Nothing is mentioned in the current ASTM standard for this material. Please advise. NozzleTwister Houston, Texas