What's The main difference between A335-P22 CL.1, CL.2 AND CL.3
regards,

Mehdi Orojlu
 
Replies continue below

Recommended for you

Where did you get these Class designations?

To my knowledge there are no Class designations associated with A335-P22. Nothing is mentioned in the current ASTM standard for this material.

Please advise.

NozzleTwister