Does anyone know of a good conversion material similar to SA-387 Gr 11 in AISI/SAE OR know of someone in the states who supplies this material?
 
Replies continue below

Recommended for you

There is no SAE equivalent because this is a steel for elevated temperature use. What quantities do you need?

Regards,

Cory

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
This is an ASME pressure vessel grade of steel plate in the US. You can try Castle Metals or Arcelor Mittal Group.
 