Mar 11, 2005 #1 soya Mechanical Joined Dec 9, 2004 Messages 11 Location GB Dear friends, May I know where to get the AISI 4340 alloy steel thermal properties? Thanks.
Mar 11, 2005 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US http://www.matweb.com/search/SpecificMaterial.asp?bassnum=M434AA Upvote 0 Downvote
Mar 11, 2005 #3 Carburize Materials Joined Sep 23, 2002 Messages 702 Location US Do you have a copy of "Smithell's Metals Reference Book" available - the data is in there. Upvote 0 Downvote
Mar 14, 2005 #4 EdStainless Materials Joined May 20, 2004 Messages 16,377 Location Waukesha WI USA Which do you need? I can look most of them up for you from a ASM ref book. I need the property and temperature of interest. = = = = = = = = = = = = = = = = = = = = Corrosion never sleeps, but it can be managed. http://www.trenttube.com/Trent/tech_form.htm Upvote 0 Downvote
Which do you need? I can look most of them up for you from a ASM ref book. I need the property and temperature of interest. = = = = = = = = = = = = = = = = = = = = Corrosion never sleeps, but it can be managed. http://www.trenttube.com/Trent/tech_form.htm