Air velocity for powder transfer through pipes

Status
Not open for further replies.

bif

Chemical
May 6, 2003
32
I am after some rule of thumb design info looking at recommended air velocity requirements for transporting powder through pipes,

The application is for a a system where material is fed off a vibrator in air, rather than coming in a compacted form

I have a recollection of using 15 - 25 m/s as a velocity and an air:powder mass ratio of between 20:1 and 10:1 respectively a few years ago on another job, but can't find any of my old references, just to check I am in the right ball park.

Thanks
 
Replies continue below

Recommended for you

Gas velocity should be above "saltation velocity" but going to high will cause erosion (abrasion) in your pipeline (mostly bends). Try to find recommended velocities for your material, but be careful - recommended values are safe as long as your powder's morphology (particle shape) and size distribution are close to the morphology and PSD of the material that the recommendation is based on.
Another link
Nick
 
blf..

Search for information, white papers etc. under the topic of "pneumatic conveying".

There seem to be no rules of thumb in this field..

The cheapest decision may be to have a sample tested...

Try "dynamic air"
Let us know what you decide..

-MJC
 