jakaodrz
Industrial
- Jun 1, 2005
- 25
I have a question.
We are using 2 tanks with medium capcity for air storing. Both are zinc plated inside to prevent corrosion.Untill 5 months ago, the capacity of our compressor was enough to satisfy our demands (Rallye 086 compressor).
Unfortunately capacity of production is going up, so the consumption of air is raising. Parallel with growth of our production we started (a few years ago installed) cleaning staion type Ultrafilter Ultrapack HED0384, year of production 1998. It is new one, and it is working fine.
Unfortunetely the working hours of our compressor are rising rapidly, because the capacity of air tanks at this moment are not enough for satisfy the consumption of air in production area and of HED0384.
As a left of a previous compressed line we have another air tank with big capacity, but it is not zinc plated inside. I'm planning to connect it to existing line but I do not know is it possible during pharmaceutical needs for clean air.
Our production is class 100.000 so maybe there should't be any problems to assure needed additional air supply , and to reduce working ours of our air compresor.
Any suggestions not to use this existing air tank ?
We are using 2 tanks with medium capcity for air storing. Both are zinc plated inside to prevent corrosion.Untill 5 months ago, the capacity of our compressor was enough to satisfy our demands (Rallye 086 compressor).
Unfortunately capacity of production is going up, so the consumption of air is raising. Parallel with growth of our production we started (a few years ago installed) cleaning staion type Ultrafilter Ultrapack HED0384, year of production 1998. It is new one, and it is working fine.
Unfortunetely the working hours of our compressor are rising rapidly, because the capacity of air tanks at this moment are not enough for satisfy the consumption of air in production area and of HED0384.
As a left of a previous compressed line we have another air tank with big capacity, but it is not zinc plated inside. I'm planning to connect it to existing line but I do not know is it possible during pharmaceutical needs for clean air.
Our production is class 100.000 so maybe there should't be any problems to assure needed additional air supply , and to reduce working ours of our air compresor.
Any suggestions not to use this existing air tank ?