Hi All!
Something I've never had to do so a little lost on who is responsible. I'm specifying a concrete mis with 6% air entrainment but the batch plant is only offering a mix of 2% and won't provide an air entrainment add mix design. The concrete contractor says he won't add a the mix in the field without guidance and testing. I can get the testing done on site by a 3rd party inspector, but can I expect the inspector to give direction on how much admix to use? Would this fall back on me as the SEOR? Thanks in advance!
Something I've never had to do so a little lost on who is responsible. I'm specifying a concrete mis with 6% air entrainment but the batch plant is only offering a mix of 2% and won't provide an air entrainment add mix design. The concrete contractor says he won't add a the mix in the field without guidance and testing. I can get the testing done on site by a 3rd party inspector, but can I expect the inspector to give direction on how much admix to use? Would this fall back on me as the SEOR? Thanks in advance!