AMS2770D seems very clear. in table VI, 7075 lists temper b4 aging T6, 250F for 8-10 hr, temper after aging, T73.
AMS2770H confuses me a little. in table 7, 7057 starts at AQ (as quenched) and W (solution heat treated). but note 4, says step 1 may be omitted if parts in T6 temper.
the parts are already made from T651 bar. it should be T7351. solution heat treat will damage/distort the parts. just want to make sure, it can be done by 250F 10 hr from T651 to T7351.
thanks.