Can anyone suggest me an adhesive for bonding inox steel? Adhesive would work in high temperature conditions. Joint strength will be important, I am looking for a simple method of making structural joints without welding.
Is there, in an Internet website, a company that produces this type of adhesive?
Many thanks in advance.



Eng. Antonino Nicosia
Aeronautical Engineer specialized in Fluid Power field.

my website: web.tiscali.it/aeronavigandosulweb
(in the future there will be many programs about fluid power problems, thermal and structural problems)
 
Replies continue below

Recommended for you

Excuse me
inox is called in English stainless

Eng. Antonino Nicosia
Aeronautical Engineer specialized in Fluid Power field.

my website: web.tiscali.it/aeronavigandosulweb
(in the future there will be many programs about fluid power problems, thermal and structural problems)
 
What is your definition of high temperature>

Epoxy-based adhesive would work up to ~ 200 [°]C.


For higher temperatures, you should consider brazing. For example, here are some silver brazes for stainless steel:


Regards,

Cory