Jul 16, 2007 #1 fralupo Materials Joined Jul 16, 2007 Messages 3 Location IT Hy,this's my question: What's the effect of pH in rubber adhesion to steel cord, is there some correlation between zinc sulfide formation ?? thank
Hy,this's my question: What's the effect of pH in rubber adhesion to steel cord, is there some correlation between zinc sulfide formation ?? thank
Jul 16, 2007 1 #2 GrahamBennett Materials Joined Feb 1, 2007 Messages 1,308 Location GB Most black-filled rubber compounds are alkaline unless they also contain silica in which case they would be pH neutral or slightly acid. As far as I know, pH does not affect the formation of ZnS. Upvote 0 Downvote
Most black-filled rubber compounds are alkaline unless they also contain silica in which case they would be pH neutral or slightly acid. As far as I know, pH does not affect the formation of ZnS.