Acrylic Pressure Vessel - Cast or Extruded?

Status
Not open for further replies.

Tanderm

Bioengineer
Dec 23, 2003
1
I'm designing a 10" OD, 20" long vessel that will see a repetitive internal vacuum load of up to 19 inHg. I've already decided on Acrylic but is cast or extruded acrylic the preferred material in this instance?
 
Replies continue below

Recommended for you

True cast acrylic has significantly better mechanical properties than extruded material and somewhat better than the so called cast material that is actually reaction extruded.