The coefficient of friction will depend on whether you have cut threads, or rolled threads, and depends on the lubrication used.<br><br>In general, a greased rolled steel thread with a steel nut (tapped thread) would have a coefficient of friction of approx. .13. Using a brass nut with a tapped thread would be about .11.