Jun 7, 2007 #1 tdjones Mechanical Joined Jun 7, 2007 Messages 1 Location US If I cut an 11-7/8" 6 stub acme-2g-lh double lead external thread will it screw into an 11-7/8" 6 stub acme single lead internal thread twice as fast? Thanks
If I cut an 11-7/8" 6 stub acme-2g-lh double lead external thread will it screw into an 11-7/8" 6 stub acme single lead internal thread twice as fast? Thanks
Jun 7, 2007 #2 eromlignod Mechanical Joined Jul 28, 2006 Messages 402 No. The internal thread has to also have two starts or the parts won't mate. The two starts are independent helixes and each must have its own independent path through the nut. Don Kansas City Upvote 0 Downvote
No. The internal thread has to also have two starts or the parts won't mate. The two starts are independent helixes and each must have its own independent path through the nut. Don Kansas City