Dear Sir,
Anyone help me to explain RT acceptance criteria for pqr and welder per aws d1.1, the statement only refer to section 6 part C, while it has some kínds of category,
4.9.2.1 RT or UT. Either RT or UT shall be used.
The entire length of the weld in test plates, except the discard lengths at each end, shall be examined in conformance with Clause 6, Part E or F. For tubulars, thefull circumference of the completed weld shall be examined in conformance with Clause 6, Part C.
Thanks