Many a times we find surface breaking defects in castings after machining at the valve manufacturer location.
These castings would have been radiographically tested(only critical area as per B16.34) and accepted with 3.2 certification.
What is the acceptance criteria for relevant indications noticed during PT/MPT on machined surfaces of castings?
Is it allowed to repair such defects, revealed by surface NDE after final machining, by welding at valve manufacturer's place? Will it affect the 3.2 certification issued by the foundry and endorsed by TPI?
These castings would have been radiographically tested(only critical area as per B16.34) and accepted with 3.2 certification.
What is the acceptance criteria for relevant indications noticed during PT/MPT on machined surfaces of castings?
Is it allowed to repair such defects, revealed by surface NDE after final machining, by welding at valve manufacturer's place? Will it affect the 3.2 certification issued by the foundry and endorsed by TPI?