Hi everybody,
Now, we encountered with internal corrosion at Valve that damage the facing of flange as attached photo's but the problem is We can not find the Reference code or recommend best practice for Acceptance or Rejection these valve due to gasket contacting surface was corroded. anyone experience to this problem, please advise. What criteria shall be use for reference.
for this cased: approximate 40% of gasket contacting surface was corroded.
Thanks for any help
Now, we encountered with internal corrosion at Valve that damage the facing of flange as attached photo's but the problem is We can not find the Reference code or recommend best practice for Acceptance or Rejection these valve due to gasket contacting surface was corroded. anyone experience to this problem, please advise. What criteria shall be use for reference.
for this cased: approximate 40% of gasket contacting surface was corroded.