mtchufi
Electrical
- Oct 3, 2003
- 23
Please help my problem, Thanks
I've several AC motor on my production line used for cutting the edge of ceramic corner (grinding), one of them has broken and I've already repaired in whork shop of motor rewinder. The problem is, after rewinded and installed to the machine, the thermal protector is always trips after several minutes started. Here is the data of the motor:
V=380 V 3 phase, Amph = 43 A
Kw = 22KW, HP = 30, Rpm=2880 , Hz = 50 Hz
When the motor started, its seem normaly, the current normal after started is about 12 Amp. but after the load applied the current rise up to 50 Amps and more. I compared with other motor, the other motor is, after started 12 A, and when loaded, its about 32 Amps. why??? thanks your help.
for addional info: the current was normal after I change the motor. The mechanical properties dosn look any problem. Try to rewind again..the problem is still same..some one can help me ??
I've several AC motor on my production line used for cutting the edge of ceramic corner (grinding), one of them has broken and I've already repaired in whork shop of motor rewinder. The problem is, after rewinded and installed to the machine, the thermal protector is always trips after several minutes started. Here is the data of the motor:
V=380 V 3 phase, Amph = 43 A
Kw = 22KW, HP = 30, Rpm=2880 , Hz = 50 Hz
When the motor started, its seem normaly, the current normal after started is about 12 Amp. but after the load applied the current rise up to 50 Amps and more. I compared with other motor, the other motor is, after started 12 A, and when loaded, its about 32 Amps. why??? thanks your help.
for addional info: the current was normal after I change the motor. The mechanical properties dosn look any problem. Try to rewind again..the problem is still same..some one can help me ??