Hi,
I have a cusotmer who is making white ABS marine speaker grilles - they are yellowing in use. The Asian vendor is mixing in his own UV stabizer (0.48%). I assume this is not the way to do it. Rather, buy a ABS UV stabilzed molding compound that has proper uV ratings. Anyone provide some advice and even some brand name compounds that can do this? The standard these is the ASTM 600 hr UV test.
Thanks
TedT
I have a cusotmer who is making white ABS marine speaker grilles - they are yellowing in use. The Asian vendor is mixing in his own UV stabizer (0.48%). I assume this is not the way to do it. Rather, buy a ABS UV stabilzed molding compound that has proper uV ratings. Anyone provide some advice and even some brand name compounds that can do this? The standard these is the ASTM 600 hr UV test.