I was reviewing a set of bridge plans and there was a note that stated all existing steel would be "abrasive blasted to a SA-1." Any ideas on what SA-1 is referring to? Is this referring to a specification on abrasive blasting or a surface finish.
 
Replies continue below

Recommended for you

This page shows some different blast standards including an SSI-SA1, which is shown being equivalent to brush-off blast. I don't know what the SSI stands for. I also find at least one reference to an ISO-SA1, but don't find an ISO standard by that name:

 