Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations LittleInch on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

ABAQUS Simple Pull out Test

Status
Not open for further replies.

BenWu

Structural
Joined
May 4, 2014
Messages
4
Location
US
Hi,

Model:

I am modeling a simple pull out test, 30 inch diameter by 20 in tall concrete cyclinder, with a 25 inch steel rebar embedded 5 inch into the concrete cylinder. The goal is to see evaluate the stresses of the embeded region for both the concrete and steel rebar. Ultimately, I would try to incorporate the damage concrete plastic model, but that is after I figure this out.

Constraints:

I used the embed funtion to embed the rebar (slave element) 5 inches into the concrete element (master element), fixed the cyclinder along the edges. The concrete is modeled as 3-D stress element while the rebar is a truss.

Loading:

A 10 kip load is applied at the endpoint of the rebar, away from the concrete cylinder.

Steps:

An initial steps and a 1 second loading step with initial increment of 0.0001


Error/Warning messages:

***WARNING: THE STRAIN INCREMENT HAS EXCEEDED FIFTY TIMES THE STRAIN TO CAUSE

FIRST YIELD AT 22 POINTS

***WARNING: THE STRAIN INCREMENT IS SO LARGE THAT THE PROGRAM WILL NOT ATTEMPT

THE PLASTICITY CALCULATION AT 8 POINTS

***NOTE: MATERIAL CALCULATIONS FAILED TO CONVERGE OR WERE NOT ATTEMPTED AT ONE

OR MORE POINTS. CONVERGENCE IS JUDGED UNLIKELY.

***ERROR: TOO MANY ATTEMPTS MADE FOR THIS INCREMENT



Methods:

I have tried partitioning the rebar into 2 sections, embedding only the 5 inches that using the embed command. I have tried it as 1 whole section, and tried with 2 separate parts - instanced the embeded 5 inch part to the concrete, and tied the endpoints of the embedded rebar to another 15 inch rebar, and then apply a 10 kip load to the endpoint of the 15 inch rebar.

I have tried making the initial increments smaller: from 0.0001 to 0.000001, but not not avail.


Material (kips):


Steel

Elastic: E=29,000 v = 0.3

Plastic:

0.0010

600.0023

60.10.015

72.50.05

77.50.1

77.90.15

72.50.175

650.183


Concrete

Density: 8.68056E-005

Elastic: E = 4.99, v=0.2

Plastic:

1.650

2.450.0005

30.0011

4.50.0035

4.40.0059

3.90.0089

3.30.0145

2.80.0195

2.40.0245

20.0295

0.40.0495



Any Suggestions or comments? Thanks!