I was wondering if there is a status output request for yield in abaqus explicit (yielded(1) or not(0)). I use Mises stress to check yield but I just wonder if there are other ways to check it.
 
In Abaqus/Standard you can use PEEQ, PEMAG and AC YIELD (the last one is a yes/no flag that you are talking about). In case of Explicit you are generally limited to PEEQ.
 