Feb 7, 2017 #1 m.wasif Mechanical Joined Jan 1, 2017 Messages 40 Location PK Can I use A105 instead of A-516 Gr70 for heat exchanger channel head cover plate and for support plate of tube bundle. Is it possible or better to replace A-516 Gr70 with A105 ??
Can I use A105 instead of A-516 Gr70 for heat exchanger channel head cover plate and for support plate of tube bundle. Is it possible or better to replace A-516 Gr70 with A105 ??
Feb 8, 2017 #2 weldstan Materials Joined Jun 24, 2011 Messages 2,809 Location US Forgings can be used. Upvote 0 Downvote